2. The wall thickness of the beam is reduced from 0.8mm/ 1.0mm to 0.3mm and 0.4 mm. Because the beam is too soft, the four sides of the floor are inclined, which seriously leads to the floor falling off and cracking.
3. Cut corners on the thickness of anti-static veneer. The standard thickness needs 0.8 mm/1.0 mm/1.2mm/1.5 mm in the south, and1.2 mm or more in the north. Poor anti-static floor can't reach this thickness naturally, which directly leads to short service life of anti-static floor.
4. The thickness of the steel plate and the pipe wall of the bracket is reduced to varying degrees, which leads to serious quality problems such as the click sound of the back and even the collapse and cracking of the floor.
5. The anti-static veneer can't meet the anti-static specification, that is, the resistance value of the anti-static system of veneer can't reach1x105 ~1x109 ohm, so the floor is not anti-static. For details, please go to the official website of www.szldfloor.com Dingling Anti-static Floor.