2.PPS polyphenylene sulfide mold temperature120-180℃ POM mold temperature: 80~ 105C, the larger the surface, the higher it can be.
3.PE-HD high-density polyethylene mold temperature: 50~95C, PC polycarbonate mold temperature: 70~ 120C.
4.PBT polybutylene terephthalate mold temperature: 40~60C is a non-reinforced material.
5.PA6 polyamide 6 or nylon 6 mold temperature: 80~90C is suitable for long-flow thin-walled plastic parts. If the wall thickness is greater than 3mm, it is recommended to use a low-temperature mold at 20 ~ 40℃ ... The mold temperature of glass reinforced materials should be higher than 80℃ ..
6. Mold temperature of 6.ABS acrylonitrile-butadiene-styrene * * * polymer: 25…70C. Mold temperature will affect the finish of plastic parts, and the lower the temperature, the lower the finish.