Artificial marble formula

an artificial marble and its manufacturing process

application number/patent number: 9812573

relates to an artificial stone, which consists of stone powder, unsaturated resin, accelerator, hardener, color powder and aluminum hydroxide powder, and the weight ratio of stone powder to unsaturated resin is 8: 2. The stone powder, resin, accelerator and hardener are mixed and stirred uniformly, and then poured. After demoulding, the surface of the product is sprayed with mixed toner and rubber shell, dried, and finally polished and waxed. The artificial marble provided by the invention is acid and alkali resistant, does not absorb water, has crystal clear texture and rich colors, and gives consideration to practicality and aesthetics. The product can be processed into basin countertops, flow countertops, coffee tables, tables and building decoration materials.