1) blanking: it is required that the size of wool is generally larger than the plate-making size, and the board surface is flat and smooth without pits.
2) Pretreatment: ① polishing, ② wire drawing, ③ treatment and ④ oxidation.
3) Water seal: After degreasing and film removal, the plate is quickly immersed in water and cannot contact with air.
Corroded metal mark
Corroded metal signs are also called etched signs. Mainly check the convex metal mark or concave metal mark made by three steps of mask and post-etching treatment. Manufacturing technology of corroded metal signs;
1) blanking: according to the size (typesetting size) required by the drawing, the edge should be added with burrs not less than 5mm around. Model 720 pedal shearing machine is used for shearing plates, which requires a flat surface and no gross profit around.